Norm
ÖNORM EN ISO 4589-3
Issue date: 1996 11 01
Plastics - Determination of burning behaviour by oxygen index - Part 3: Elevated-temperature test (ISO 4589-3:1996)
This part of IS0 4589 specifies methods for determining
the minimum concentration of oxygen, in a mixture with nitrogen, that will support combustion of small vertical t...
Withdrawn: 2017 08 15
Publisher:
Austrian Standards International
Format:
Digital | 23 Pages
Language:
German
| English
| Download GER/ENG
Currently valid:
Optionally co-design standards:
This part of IS0 4589 specifies methods for determining
the minimum concentration of oxygen, in a mixture with nitrogen, that will support combustion of small vertical test specimens under specified test conditions over a range of temperatures typically between 25 C and 150 C. The results are defined as oxygen index values at the test temperature, which is typical of the practical temperature that a plastic material may experience in an overheated service situation.
ÖNORM EN ISO 4589-3
2017 08 15
Plastics - Determination of burning behaviour by oxygen index - Part 3: Elevated-temperature test (I...
Norm
ÖNORM EN ISO 4589-3
1996 11 01
Plastics - Determination of burning behaviour by oxygen index - Part 3: Elevated-temperature test (I...
Norm
↖
Norm
Issue date :
1996 07 18
Plastics — Determination of burning behaviour by oxygen index — Part 2: Ambient-temperature test
Norm
Issue date :
2017 08 15
Plastics - Determination of burning behaviour by oxygen index - Part 3: Elevated-temperature test (ISO 4589-3:2017)
Norm
Issue date :
1996 08 08
Plastics — Determination of burning behaviour by oxygen index — Part 3: Elevated-temperature test